316 SS yeeb nkab fittings yog dab tsi?

Apr 15, 2026

Tso lus

316 SS yeeb nkab fittings yog dab tsi?

316 stainless hlau yeeb nkab fittings xa mus rau cov yeeb nkab txuas cov khoom ua los ntawm 316 stainless hlau (los yog nws ultra- qis carbon version, 316L). Lawv tau siv dav hauv kev lag luam tsheb thauj mus los rau kev ua haujlwm xws li kev sib txuas, kev hloov pauv, txoj kab uas hla hloov, sealing, lossis kaw.
Hom Hom: Xws li lub luj tshib, tees, reducers, couplings, caps, thiab unions.
Cov Qauv: Ua raws li ASTM A403, ASME B16.9, thiab B16.11.
Daim ntaub ntawv: Dav siv nyob rau hauv tshuaj ua, offshore platforms, desalination nroj tsuag, zaub mov & dej haus, thiab kws industries.

 

Durable Stainless Steel 316 Elbow
Stainless hlau 316 luj tshib
316 Stainless Steel Three Way Tee
316 Stainless Hlau Peb Txoj Kev Tee
SS 316  Pipe Fitting Reducer
SS 316 yeeb nkab haum reducer
Stainless Steel Pipe Fitting 316 Cap
Stainless hlau yeeb nkab haum 316 Cap

 

316 SS yeeb nkab haum Standards & Specifications

Qeb Yam khoom Specification / Txuj
Khoom siv (Wrought) Buttweld Fittings ASTM A403 / ASME SA403 (WP 316, WP316L, WP316H)
Khoom siv (Forged) Threaded & Socket Weld ASTM A182, ASME SA182 (F316, F316L)
Qhov ntev Buttweld Fittings ASME B16.9 (loj Bore), MSS SP-43 (Lub Teeb Nyhav)
Qhov ntev Forged Fittings ASME B16.11 (Socket Weld & Threaded)
Qhov ntev Flanges ASME B16.5 (txog 24 "), ASME B16.47 (siab dua 24")
Xov Yeeb Nkab Xov ASME B1.20.1 (NPT), ISO 7-1 (BSPT), ISO 228 (BSPP)
Cov ntawv pov thawj Cov Ntawv Qhia Zoo EN 10204 3.1 / 3.2, NACE MR0175 / ISO 15156

 

ASTM A403 / A 182 316 Tshuaj muaj pes tsawg leeg (%)

Qib Cov pa roj carbon (C) Manganese (Mn) Silicon (Si) Phosphorus (P) Sulfur (S) Chromium (Cr) Nickel (Ni) Molybdenum (hli)
316 0.08 max max 2.00 Nws max 1.00 Nws 0.045 max 0.030 max 16.0 - 18.0 10.0 - 14.0 2.00 - 3.00
316L 0.03 max max 2.00 Nws max 1.00 Nws 0.045 max 0.030 max 16.0 - 18.0 10.0 - 14.0 2.00 - 3.00

 

316 yeeb nkab Fittings Muaj Ntau Yam

Fitting Qeb Hom kev sib txuas Cov khoom siv Qhov Loj Phab ntsa Thickness / Rating
Buttweld Welded (BW) 45℃/ 90℃/ 180℃Luj tshib (LR / SR), Sib npaug / Txo Tee, Conc. / Ecc. Reducer, Cap, Stub End 1/2 "mus rau 48" SCH 5S, 10S, 40S, 80S, 160S, XXS
Forged Qhov (socket) Weld (SW) 90℃Luj tshib, Tee, Hla, Union, Coupling, Cap 1/8 "mus rau 4" Chav Kawm 3000, 6000, 9000
Forged Threaded (THD) NPT / BSPT Luj Tshib, Tee, Txoj Kev Luj Tshib, Hex Bushing, Nipple, Plug 1/8 "mus rau 4" Chav Kawm 2000, 3000, 6000
Flanges Ntau yam Weld Neck (WN), Slip-On (SO), Dig muag (BL), Lap Joint (LJ) 1/2 "mus rau 60" Chav Kawm 150 txog 2500

 

Mechanical Properties ntawm 316/316L Fittings

Cov ntaub ntawv tseem ceeb rau kev suav engineering (Pressure Vessel Code ua raws).

Khoom Qib 316 (Min. Requirement) Qib 316L (Min. Requirement)
Tensile zog (ksi / MPa) 75 / 515 70 / 485
Yield zog 0.2% Offset (ksi / MPa) 30 / 205 25 / 170
Elongation hauv 2 hauv. (%) 35% - 40% 35% - 40%
Hardness (Brinell - HBW) 187 Max 187 Max
Hardness (Rockwell - HRB) 90 Max 90 Max

 

Kev ntsuas siab rau 316 Forged Fittings (ASME B16.11)

Kev siv ceev ceev rau kev txwv siab ntawm qhov kub thiab txias.

Chav Kawm Hom Fitting Ambient Temp Service Pressure (PSI) Ambient Temp Service Siab (Bar)
Chav Kawm 2000 Xov 2,000 PSI ~ 138 Ib
Chav Kawm 3000 Xov / SW 3,000 PSI ~ 207 Ib
Chav Kawm 6000 Xov / SW 6,000 PSI ~ 414 Ib
Chav Kawm 9000 Qhov (socket) Weld 9,000 PSI ~ 620 hli

 

Dab tsi yog qhov txawv ntawm 304 thiab 316 stainless hlau fittings?

Qhov sib txawv tseem ceeb ntawm 304 thiab 316 stainless hlau yeeb nkab fittings yog 316 muaj 2-3% molybdenum, muab nws superior corrosion kuj piv rau 304, tshwj xeeb tshaj yog nyob rau hauv chloride thiab marine ib puag ncig . 304 yog haum rau dav siv, sab hauv tsev, thiab dej tshiab daim ntaub ntawv, thaum 316, vim nws cov durability ntau dua, yog zoo dua nyob rau hauv cov tshuaj chemical thiab ntsev.

 

316 SS yeeb nkab fittings tsum

GNEE muab 316 cov kav dej, fittings, flanges, li qub, thiab gaskets, kom ntseeg tau cov kev qhia tshwj xeeb thiab haum rau tag nrho cov kav dej. Peb tuaj yeem tsim cov khoom tsis yog- tus qauv luj tshib (xws li, radii tshwj xeeb) lossis loj - txoj kab uas hla, tuab- cov phab ntsa reducers raws li cov neeg siv khoom CAD kos duab.

Butt-welded fittings: Siv cov tshuab txias extrusion lossis thermoforming tshuab, kom ntseeg tau tias cov phab ntsa tuab tuab thiab cov beveling tiav rau qhov yooj yim automated ntawm - qhov chaw vuam.

Forged fittings: Forged siv siab -tonnage forging presses, ua rau cov hlau ntws ua tiav, tshem tawm cov porosity thiab tawg, thiab muaj peev xwm tiv taus qhov system siab heev.

Kev them nyiaj yug daim ntawv pov thawj: Muab ua tiav MTC (Cov ntaub ntawv pov thawj ntawm kev ua raws) raws li EN 10204 3.1.

 

GNEE 316/316L Stainless Hlau Yeeb Fittings Khoom Ntau

Peb muab tag nrho ntau yam ntawmButtweld, Socket Weld, thiab Threaded fittings, npog ntau yam kev siv hauv kev lag luam.

Qeb Cov khoom siv Cov qauv Qhov Loj Phab ntsa Thickness / Siab ntsuas
Buttweld Fittings 90℃/ 45℃Luj tshib, sib npaug / Txo Tees, Reducers (Concentric / Eccentric), Yeeb Nkab Cap, Stub Ends ASME B16.9, MSS SP-43, EN 10253 1/2 "- 48" (Seamless / Welded) SCH 5S, 10S, 40S, 80S, 160S, XXS
Forged Fittings (Socket Weld) Socket Weld Luj Tshib, Tees, Hla, Unions, Couplings, Olets ASME B16.11, BS 3799 1/8" – 4" 3000#, 6000#, 9000#
Xov Fittings NPT / BSPT Luj tshib, Threaded Tees, Hex Nipples, Bushings, Plugs ASME B16.11, ISO 4144 1/8" – 4" 150#, 2000#, 3000#
Flanges Slip-On (SO), Weld Neck (WN), Dig muag (BL), Socket Weld (SW) ASME B16.5, EN 1092-1 1/2" – 60" Chav Kawm 150 - 2500, PN6 - PN160

 

Hu rau tam sim no

 

316/316L Stainless Steel Pipe Fittings
316/316L Stainless Steel Pipe Fittings
 

Xa kev nug