Dab tsi yog 2507 stainless hlau?
Feb 25, 2026
Tso lus



Tshuaj muaj pes tsawg leeg
Cov tshuaj muaj pes tsawg leeg ntawm stainless hlau qib Super Duplex 2507 yog teev nyob rau hauv cov lus hauv qab no.
| Element | Cov ntsiab lus (%) |
|---|---|
| Chromium, Cr | 24 – 26 |
| Nickel, Nia | 6 – 8 |
| Molybdenum, Mo | 3 – 5 |
| Manganese, Mn | 1.20 max |
| Silicon, Sib | 0.80 max |
| tooj, Cu | 0.50 max |
| Nitrogen, N | 0.24 – 0.32 |
| Phosphorus, P | 0.035 max |
| Carbon, C | 0.030 max |
| Sulfur, S | 0.020 max |
| Hlau, Fe | Tshuav |
Lub cev muaj zog
Lub cev lub cev ntawm stainless hlau qib Super Duplex 2507 yog tabulated hauv qab no.
| Cov khoom | Metric | Imperial |
|---|---|---|
| Qhov ntom | 7.8g / cm33 | 0.281 lb/in3 |
| Melting point | 1350 degree | 2460℃F |
Xa kev nug