Dab tsi yog 1.4315 stainless hlau sib npaug?

Mar 13, 2026

Tso lus

Dab tsi yog 1.4315 stainless hlau?

1.4315 (X5CrNiN19-9) yog ib qho austenitic stainless hlau txhim kho nrog nitrogen kom muaj zog dua thiab txhim kho corrosion kuj piv rau cov qauv 304/1.4301 qib. Raws li cov khoom siv ruaj khov, nitrogen-alloyed, thiab feem ntau tsis yog- cov khoom siv hlau nplaum, feem ntau yog siv rau hauv cov khoom siv tshuaj, cov cuab yeej kho mob, thiab cov ntawv siv siab.

 

Dab tsi yog 1.4315 stainless hlau sib npaug?

1.4315 stainless hlau (X5CrNiN19-9) feem ntau yog sib npaug rau AISI 304N (UNS S30451). Nws yog nitrogen-alloyed, austenitic stainless hlau paub txog lub zog ntau dua thiab txhim kho corrosion kuj piv rau tus qauv 304/1.4301, feem ntau yog siv rau fasteners, springs, thiab structural applications.

 

Cov tshuaj muaj pes tsawg leeg ntawm steel X5CrNiN19-9 (1.4315): EN 10088-2-2005

Cov ntsiab lus tsis tau teev nyob rau hauv cov lus no yuav tsum tsis txhob txhob txwm muab ntxiv rau cov hlau yam tsis muaj kev pom zoo ntawm tus neeg yuav khoom tshwj tsis yog ua kom tiav cov cam khwb cia.
C Si Mn Ni P S Cr N
max 0.06 max1 ua max2 ua 8 - 11 max 0.045 Nws max 0.015 18 - 20 0.12 - 0.22

 

Mechanical Properties ntawm Steel X5CrNiN19-9 (1.4315)

X5CrNiN19-9 (EN 1.4315) yog ib qhoaustenitic chromium-nickel stainless hlau nrog nitrogen ntxiv, muab lub zog siab dua li cov qib ib txwm zoo li 304 thaum tuav cov kev tiv thaiv zoo heev thiab kev tsim kho.

Khoom Tus nqi Chav tsev
Tensile zog (Rm) 650 – 880 MPa
Yield zog (Rp0.2) Ntau dua lossis sib npaug li 350 MPa
Elongation (A) Ntau dua lossis sib npaug li 40 %
Hardness (HB) Tsawg dua lossis sib npaug li 215 HB
Hardness (HRB) Tsawg dua los yog sib npaug li 95 HRB
Modulus ntawm Elasticity 193 GPa
Impact Toughness (Charpy V) Ntau dua los yog sib npaug rau 100 J
Kev qaug zog ~240 MPa

 

Dab tsi yog qhov txawv ntawm 1.4315 thiab 1.4301 stainless hlau?

Ob leeg 1.4301 thiab 1.4315 yog austenitic stainless hlau nrog cov ntsiab lus zoo sib xws (muaj 18-19% chromium thiab 8-10% nickel); Txawm li cas los xij, qhov sib txawv ntawm ob yog tias 1.4315 (X5CrNiN19-9) tau dhau los ntawm nitrogen alloying, ua rau muaj zog dua piv rau tus qauv 1.4301 (X5CrNi18-10, piv txwv li, AISI 304).

 

Dab tsi yog qhov txawv ntawm 1.4315 thiab 1.4307 stainless hlau?

Ob leeg EN 1.4307 (304L) thiab 1.4315 (X5CrNiN19-9) yog austenitic stainless hlau; tshwj xeeb, 1.4315 nthuav tawm lub zog ntau dua vim qhov sib ntxiv ntawm nitrogen ua cov khoom siv alloying, whereas 1.4307 (cov pa roj carbon tsawg) yog qhov zoo dua rau kev vuam . 1.4307 qhia tau zoo heev corrosion kuj thiab tshwj xeeb tshaj yog haum rau welded Cheebtsam; Hauv qhov sib piv, 1.4315 feem ntau yog xaiv thaum lub zog ntawm cov qauv kev xav tau ntau dua.

 

1.4315 Stainless Hlau: Corrosion Resistance

1.4315 (X5CrNiN19-9) yog austenitic stainless hlau nrog zoo corrosion kuj, superior rau qib 302 vim nws cov nitrogen-alloyed muaj pes tsawg leeg. Nws muaj kev ua haujlwm zoo hauv oxidizing ib puag ncig, siab tensile zog, thiab zoo weldability. Nws yog dav siv rau fasteners nyob rau hauv me me corrosive ib puag ncig.


1.4315 Stainless hlau: Machinability

1.4315 (X5CrNiN19-9) yog ib qho austenitic stainless hlau nrog nruab nrab machinability, feem ntau zoo ib yam li los yog me ntsis nyuaj rau lub tshuab dua Qib 304 vim siab nickel thiab nitrogen cov ntsiab lus, uas ua rau kom toughness thiab ua hauj lwm hardening. Nws nquag siv rau forged, siab - lub zog qhov chaw es tsis siv lub tshuab ua haujlwm siab ceev.


Puas yog 1.4315 stainless hlau sib nqus?

1.4315 (X5CrNiN19-9) yog ib qho austenitic stainless hlau uas feem ntau tsis sib nqus hauv nws lub xeev annealed. Txawm li cas los xij, vim nws muaj pes tsawg leeg, nws tuaj yeem tsim cov khoom sib nqus me ntsis thaum raug ua haujlwm txias, xws li khoov, dov, lossis kos duab.

 

Gnee muaj ntau yam khoom siv hauv qib 1.4315 (AISI 304N) cov ntaub ntawv, suav nrog nruab nrab- rau- cov phaj hnyav, txias- dov coils, siab- cov kav dej tsis sib haum, cov kav dej muaj welded, cov kav dej sib txuas, thiab lwm yam. Peb qhov kev sib tw tseem ceeb yog los ntawm kev sib sib zog nqus kev koom tes nrog rau sab saum toj -tier steel mills- xws li TISCO thiab Baosteel- kom ntseeg tau 100% cov ntaub ntawv traceability thiab 100% PMI (Positive Material Identification) spectral testing. Kev txhawb nqa los ntawm peb hauv -cov chaw hauv tsev muab ib qho - nres laser txiav, precision dabtsi yog khoov, thiab cov kev pabcuam nto tiav, peb xa cov khoom lag luam zoo tshaj plaws rau lub nkoj thoob ntiaj teb, cryogenic engineering, thiab cov khoom siv tshuaj lom neeg- sib txuas ua haujlwm tau zoo nrog kev xa khoom sai thoob ntiaj teb.

1.4315 (AISI 304N) stainless steel pipes
1.4315 (AISI 304N) stainless hlau kav
1.4315 (AISI 304N) stainless steel coils
1.4315 (AISI 304N) stainless hlau coils