UNS S40900 yog ib qho qis -chromium, titanium- ruaj khov ferritic stainless hlau renowned rau nws cov nqi zoo heev - kev ua tau zoo piv thiab txhim khu kev qha siab - kub oxidation kuj. Raws li qib ferritic, nws nthuav tawm cov khoom sib nqus thiab cov thermal conductivity zoo, qhov txawv ntawm nws tus kheej los ntawm austenitic stainless hlau. Lub titanium ntxiv stabilizes cov hlau, tiv thaiv intergranular corrosion thiab txhim kho weldability, ua rau nws yooj yim rau fabricate ntawm txiav, sib sau, thiab vuam txheej txheem. Nws feem ntau yog tsim los rau cov ntawv thov uas xav tau kev tiv thaiv corrosion nruab nrab thiab siab - qhov kub thiab txias, ua haujlwm raws li tus nqi - kev daws teeb meem zoo hauv kev lag luam tsheb thiab kev lag luam dav dav uas cov peev nyiaj thiab kev ua tau zoo yog qhov tseem ceeb.

Chemical Composition (wt%)

C Less tshaj los yog sib npaug 0.08, Cr: 10.50-11.75, Ti: 0.15-0.35, Mn Less tshaj los yog sib npaug rau 1.00, Si Less tshaj los yog sib npaug rau 1.00, P Less dua los yog sib npaug rau 0.045, S Less dua los yog sib npaug rau 0.050 los yog sib npaug rau Ni 0.030 Nws

Tej yam cuab yeej cuab tam (Annealed Condition)

Tensile Strength (Rm): Ntau dua lossis sib npaug li 448 MPa; Yield zog (Rp0.2): Ntau dua lossis sib npaug rau 238 MPa; Elongation (A): Ntau dua lossis sib npaug li 33%; Brinell Hardness (HB): Tsawg dua lossis sib npaug rau 183

Core Zoo

Tus nqi -zoo nrog rau kev tiv thaiv corrosion; titanium stabilization tiv thaiv intergranular corrosion thiab txhim kho weldability; zoo heev - kub oxidation kuj (txog 760 degree); zoo formability zoo ib yam li carbon steel; sib nqus nrog siab thermal conductivity; haum rau kev tsim khoom loj nrog cov khoom siv qis.

Daim ntawv thov

Automotive tso tshuab (manifolds, mufflers, tailpipes, catalytic converters), lub tsev cua sov tshuab, cua sov exchanger tubing, hluav taws xob transformer rooj plaub, architectural trim, thiab kev lag luam feem ntau nyob rau hauv me me corrosive ib puag ncig.

Qib sib npaug

EN 1.4512, AISI 409, GB 022Cr11Ti, SUS409L

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj hauv Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI xeem tsab ntawv ceeb toom, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips

Xa kev nug