Apr 13, 2026
Tso lus




Cov khoom tseem ceeb
Cov ntu hauv qab no yuav tham txog cov khoom ntawm qib 416 steel bar khoom ntawm ASTM A582. Cov khoom tshwj xeeb yuav tsis zoo ib yam li lwm cov ntaub ntawv xws li forgings thiab xov hlau.
Kev sib xyaw
Cov tshuaj muaj pes tsawg leeg ntawm qib 416 stainless hlau tau muab rau hauv cov lus hauv qab no:
Table 1 - Kev sib xyaw ua ke rau qib 416 stainless hlau
Qib | C | Mn | Si | P | S | Cr | Mo | |
416 | min. max. | - 0.15 | - 1.25 | - 1 | - 0.06 | 0.15 - | 12 14 | - 0.6 |
Mechanical Properties
Cov lus hauv qab no muab cov khoom siv kho tshuab ntawm qib 416 stainless hlau:
Table 2 - Mechanical zog ntawm qib 416 stainless hlau
Tempering Kub (°C) | Tensile zog (MPa) | Yield zog | Elongation | Hardness Brinell | Impact Charpy V (J) |
Annealed * | 517 | 275 | 30 | 262 | - |
Qhov xwm txheej T ** | 758 | 586 | 18 | 248-302 | - |
204 | 1340 | 1050 | 11 | 388 | 20 |
316 | 1350 | 1060 | 12 | 388 | 22 |
427 | 1405 | 1110 | 11 | 401 | # |
538 | 1000 | 795 | 13 | 321 | # |
593 | 840 | 705 | 19 | 248 | 27 |
650 | 796 | 670 | 17.5 | 253 | 38 |
* Annealed cov khoom yog ib yam rau cov mob A ntawm ASTM A582.
** Hardened thiab tempered Condition T ntawm ASTM A 582 - Brinell hardness yog teev ntau yam, lwm yam khoom yog ib yam nkaus xwb.
#Tempering ntawm cov hlau no ntawm qhov kub ntawm 400 txog 580 ° C yuav tsum tau zam vim muaj kev cuam tshuam tsis zoo.
Lub cev muaj zog
Lub cev tseem ceeb ntawm annealed qib 416 stainless hlau yog tabulated hauv qab no:
Table 3 - Lub cev muaj zog ntawm annealed qib 416 stainless hlau
Qib | Qhov ceev (kg / m3) | Elastic Modulus (GPa) | Lub ntsiab lus Coefficient ntawm Thermal Expansion | Thermal conductivity | Tshwj xeeb kub 0-100°C | Hluav taws xob tiv thaiv (nΩ) | |||
0-100 ° C | 0-315 ° C | 0-538 ° C | ntawm 100 ° C | ntawm 500 ° C | |||||
416 | 7800 | 200 | 9.9 | 11 | 11.5 | 24.9 | 28.7 | 460 | 570 |
Xa kev nug