SUS631 Stainless hlau: nag lossis daus-Nruj rau cov ntawv thov caij nplooj ntoos hlav

Jan 22, 2026

Tso lus

SUS316L Stainless Steel: Low-Carbon Corrosion Resistant Grade304 Stainless Steel Round Bar and tubeSTAINLESS STEEL SHEET

Cov khoom tseem ceeb rau Springs

Siab zog & Hardness:Ua tau zoo heev mechanical zog tom qab kev laus kho, txhawb nqa ntau dua.

Zoo Fatigue Resistance:Tiv thaiv rov qab kev ntxhov siab, tiv thaiv kev ua tsis tiav ntxov hauv kev siv dynamic.

Zoo Corrosion Resistance:Tswj kev ua tau zoo hauv qhov hnyav lossis corrosive qhov twg cov qauv hlau yuav ua tsis tau.

Formability:Muab zoo formability ua ntej hardening, enabling complex caij nplooj ntoos hlav duab.

Temperature Stability:Ua tau zoo ntawm qhov kub siab, txog li 315 ° C (600 ° F).

Nws ua haujlwm li cas (Precipitation Hardening)

Kev Kho Mob:Cov khoom yog rhuab thiab ces txias txias (quenched) los tuav nws alloying ntsiab nyob rau hauv cov khoom tov, ua rau nws mos thiab formable.

Kev laus (Precipitation):Kev kho cua sov tom qab (kev laus) nyob ib puag ncig 480 ° C (896 ° F) ua rau cov dej sib xyaw ua ke zoo (xws li Ni3Al) tsim nyob rau hauv cov hlau cov qauv, ua rau nws lub zog thiab hardness.

Common Spring Applications

Aerospace:Cheebtsam xav tau lub zog siab - rau - qhov hnyav piv thiab kev ntseeg tau.

Electronics:Pogo pins, connectors, thiab precision springs hauv cov khoom siv.

Automotive:Cheebtsam xav tau durability thiab resilience.

Cov cuab yeej kho mob:Qhov twg precision, corrosion kuj, thiab lub zog tseem ceeb heev.

Daim ntawv muaj

Hlau (rau coil springs)

Ntawv nyiaj (rau precision springs, diaphragms)

Sheet & Sawb (rau tiaj tus springs, bellows)