SUS430 - Economical Ferritic Alloy Rau Kho Kom Zoo Nkauj & Muaj Kev Siv Ua Haujlwm

Mar 30, 2026

Tso lus

Txheej txheem cej luam

SUS430 yog cov khoom siv dav siv ferritic stainless hlau tau teev tseg los ntawm JIS G 4303 / G 4304, featuring 16.00-18.00% chromium rau huab cua zoo thiab dej tsis qab corrosion. Raws li tsis yog-kub- qib kho tau, nws tswj cov khoom siv kho tshuab ruaj khov thiab muaj cov qauv zoo heev, ua rau nws yooj yim rau stamp, khoov, thiab vuam. Nws yog hlau nplaum, muaj lub ntuj matte tiav uas polishes zoo, thiab yog tus nqi -zoo-txoj haujlwm nws yog qhov kev xaiv nrov rau kev siv kho kom zoo nkauj thiab kev lag luam dav dav uas kev zoo nkauj thiab nyiaj txiag yog qhov tseem ceeb. Tsis zoo li cov qib austenitic, nws tiv taus chloride kev nyuaj siab corrosion tawg ntawm qhov kub siab.

Chemical Composition (wt%)

C Tsawg dua lossis sib npaug 0.12, Cr: 16.00-18.00, Mn Tsawg dua lossis sib npaug 1.00, Si Less dua lossis sib npaug 1.00, P Tsawg dua lossis sib npaug 0.040, S Less dua lossis sib npaug 0.030, Ni Less dua lossis sib npaug 0.75 Ti,

Tej yam cuab yeej cuab tam (Annealed Condition)

Tensile Strength (Rm): Ntau dua lossis sib npaug li 450 MPa; Yield zog (Rp0.2): Ntau dua lossis sib npaug rau 205 MPa; Elongation (A): Ntau dua lossis sib npaug li 22%; Brinell Hardness (HB): Tsawg dua lossis sib npaug rau 183

Core Zoo

Tus nqi -zoo nrog zoo atmospheric corrosion kuj; zoo heev formability thiab weldability; Sib nqus; yooj yim rau polish rau cov hniav tiav; non-kub- kho tau nrog cov khoom siv kho tshuab ruaj khov; superior tsis kam rau chloride kev nyuaj siab corrosion cracking piv rau austenitic qib; haum rau ntau lawm.

Daim ntawv thov

Cov khoom siv hauv tsev (cov tub yees, qhov cub), cov khoom siv hauv tsev, cov khoom siv hauv tsev, cov khoom siv hauv tsev, cov ntaub ntawv zoo nkauj, cov khoom siv hauv tsheb, cov txee, thiab cov khoom siv dav dav hauv cov cheeb tsam me me.

Qib sib npaug

EN 1.4016, UNS S43000, GB 06Cr17, AISI 430

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips

Xa kev nug