SUS316 Sheet, Phaj, Coil Specifications: Thickness, Dav, Qhov hnyav

Dec 03, 2025

Tso lus

SUS316 Sheet, Phaj, thiab Coil yog dab tsi?

SUS316 (1.4401, X5CrNiMo17-12-2) yog ib hom austenitic stainless hlau uas muaj molybdenum, uas ua rau nws muaj zog tiv thaiv corrosion. Cov khoom siv SUS316 tuaj yeem ua tiav rau hauv cov ntawv, daim hlau, thiab cov coils, nrog cov thicknesses sib txawv thiab dav xaiv raws li qhov xav tau sib txawv. Cov ntawv thov muaj xws li tshuaj lom neeg, dej hiav txwv thiab ntsev tsuag ib puag ncig, khoom siv hauv cov khoom noj thiab tshuaj lag luam, cov khoom siv hluav taws xob, cov tso tsheb hlau luam, cov kav dej thiab cov hlab ntsha, thiab kev kho kom zoo nkauj hauv tsev thiab kev tiv thaiv.

 

Dab tsi yog qhov specifications ntawm SUS316 stainless hlau ntawv?

SUS316 daim ntawv, phaj, thiab coil specifications feem ntau txhais los ntawm ASTM A240 / ASME SA240, nrog qhov ntev feem ntau yog li ntawm 4mm txog 100mm hauv tuab thiab ntau qhov ntev thiab dav xws li 2440mm, 6000mm, thiab 1000mm txog 3500mm, ntsig txog. Specifications muaj xws li txhua yam khoom (lub zog tensile: 515 MPa, yield zog: 205 MPa, elongation: 40%), thiab nto tiav xws li NO.1, 2B, BA, thiab No.4.

 

Dab tsi yog cov khoom sib npaug ntawm SUS316 Stainless Steel phaj?

Qib UNS No Laus British Euronorm Swedish SS Japanese JIS
BS En Tsis muaj Lub npe
316 S31600 316S31 58H, 58J 1.4401 X5CrNiMo17-12-2 2347 TIAB SA 316
316L S31603 316S11 - 1.4404 X2CrNiMo17-12-2 2348 SUS 316L
316H S31609 316S51 - - - - -

 

316 Stainless Steel Chemical Composition

Cov ntsiab lus (%)

316 (S31600)

316L (S31603)

Carbon, Max

0.08

0.030

Manganese, Max

2.00

2.00

Phosphorus, Max

0.045

0.045

Sulfur, Max

0.030

0.030

Silicon, Max

0.75

0.75

Chromium

16.0-18.0

16.0-18.0

Nickel

10.0-14.0

10.0-14.0

Mo

2.00-3.00

2.00-3.00

Nitrogen

0.10

...

 

316 Stainless Hlau Mechanical Properties

Mechanical Properties

316 (S31600)

304L (S30403)

Tensile zog Min

75 Ksi [515 Mpa]

70 Ksi [485 Mpa]

Yield Strength Min 0.2% offset

30 Ksi [205 Mpa]

25 Ksi [170 Mpa]

Yield Strength Min 1% offset

38 Ksi [260 Mpa]

38 Ksi [260 Mpa]

Elongation Min

40%

40%

Hardness Max

95 PAB

95 PAB

 

316 Stainless Hlau Sheet Gauge Thickness

Ntsuas 30 28 26 24 22 20 18 16
Thickness nyob rau hauv nti .0119 .0149 .0179 .0239 .0299 .0359 .0478 .0598
Thickness nyob rau hauv millimeter .3 .4 .5 .6 .8 .9 1.2 1.5

 

UNS S31600 Cold Rolled Phaj Nyhav ib square Meter

Thickness nyob rau hauv mm Qhov hnyav Kg / m2
0,40 3,144
0,60 4,716
0,80 6,288
1,00 7,860
1,20 9,432
1,50 11,790
1,80 14,148
2,00 15,720
2,50 19,650
4,00 31,440
6,00 47,160
10,00 78,600

 

Yuav ua li cas xam SUS316 phaj hnyav?

Kev xam qhov hnyav ntawm SUS316 stainless hlau phaj yog ncaj nraim yog tias koj paub nws thickness, dav, thiab ntev. Qhov ceev ntawm SUS316 yog kwv yees li 7.99 g / cm³ (los yog 7,990 kg / m³).

Qhov hnyav ntawm kev xam cov qauv

SUS316 stainless steel plate

Kauj ruam -los ntawm - kauj ruam:

Hloov thickness thiab dav mus rau meters (los yog siv qhov 0.00799 hloov mm²·m rau kg).

Muab cov thickness × dav × ntev kom tau ntim hauv cubic meters.

Muab qhov ntom ntom (7,990 kg / m³) kom tau qhov hnyav hauv kilograms.

 

ASME SA240 Qib 316 Strip Tolerance

Phaj Thickness (hauv) Tolerance (hauv) *
1-1-3/4 ib +.070 / -.010
2-2-3/4 ib +.125 / -.010
3 rau 4 +.175 / -.010
3/4 txog 15/16 +.060 / -.010
3/8 txog 11/16 +.055 / -.010
3/16 au 5/16 +.045 / -.010

 

GNEE muab cov ntawv hlau stainless, daim hlau, thiab coils hauv ntau qhov ntau thiab tsawg. Thov hu rau peb rau qhov ntau thiab tsawg los yog kev xa khoom sai.

Peb Cov Khoom Muag Khoom Muag:
Cov Qauv: ASTM A240, ASME -SA240
Thickness Ntau: 0.02mm - 4mm, 4.5mm - 100mm
Dav Dav: 900mm - 2400mm
Ntev Ntev: 3000mm - 12000mm (Stainless Steel Coils)
Deg tiav: Ntuj, 2B, Daim iav

info-600-400


Kev Pabcuam Hlau Txiav: Laser Txiav, Waterjet Txiav, Plasma Txiav

Ntim: Ntoo thawv, pallets, lossis coil wrapping rau kev nyab xeeb.

Lub sij hawm xa tuaj: 7-15 hnub nyob ntawm seb muaj pes tsawg thiab kev hloov kho.

ASME SA240 Grade 316 Strip
ASME SA240 Grade 316 plate

Xa kev nug