STS430 yog cov khoom siv dav siv ferritic stainless hlau, muaj 16.00-18.00% chromium rau cov huab cua zoo thiab dej tsis qab corrosion. Raws li tsis yog-kub- qib kho tau, nws muaj cov khoom siv kho tshuab ruaj khov thiab muaj cov qauv zoo heev, ua rau nws yooj yim rau stamp, khoov, thiab vuam. Nws yog hlau nplaum, muaj lub ntuj matte tiav uas polishes zoo, thiab yog tus nqi -zoo-txoj haujlwm nws yog qhov kev xaiv nrov rau kev siv kho kom zoo nkauj thiab kev lag luam. Tsis zoo li qib austenitic, STS430 tiv thaiv chloride kev nyuaj siab corrosion tawg ntawm qhov kub siab, ntxiv rau nws ntau yam.
Chemical Composition (wt%)
C Tsawg dua lossis sib npaug 0.12, Cr: 16.00-18.00, Mn Tsawg dua lossis sib npaug 1.00, Si Less dua lossis sib npaug 1.00, P Tsawg dua lossis sib npaug 0.040, S Less dua lossis sib npaug 0.030, Ni Less dua lossis sib npaug 0.75 Ti,
Tej yam cuab yeej cuab tam (Annealed Condition)
Tensile Strength (Rm): Ntau dua lossis sib npaug li 450 MPa; Yield zog (Rp0.2): Ntau dua lossis sib npaug rau 205 MPa; Elongation (A): Ntau dua lossis sib npaug li 22%; Brinell Hardness (HB): Tsawg dua lossis sib npaug rau 183
Core Zoo
Tus nqi - zoo nrog txhim khu kev qha atmospheric corrosion kuj; zoo heev formability thiab weldability; Sib nqus; yooj yim rau polish rau cov hniav tiav; non-kub- kho tau nrog cov khoom siv kho tshuab ruaj khov; superior tsis kam rau chloride kev nyuaj siab corrosion cracking piv rau austenitic qib; haum rau ntau lawm.
Daim ntawv thov
Cov khoom siv hauv tsev (cov tub yees, qhov cub), cov khoom siv hauv tsev, cov khoom siv hauv tsev, cov khoom siv hauv tsev, cov ntaub ntawv zoo nkauj, cov khoom siv hauv tsheb, cov txee, cov khoom siv, thiab cov khoom lag luam dav dav hauv cov cheeb tsam me me.
Qib sib npaug
EN 1.4016, UNS S43000, GB 06Cr17, AISI 430, SUS430
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj hauv Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI xeem tsab ntawv ceeb toom, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.


Xa kev nug