Stainless hlau - Qib 440 (UNS S44000)

Mar 03, 2026

Tso lus

SUS 440c Stainless Steel Plate AMS 5630 AISI 440C SS Steel PlateASTM A240 AISI 904L UNS N08904 1.4539 S39042 Hot Rolled Stainless Steel Plate304L Stainless Steel Sheet for Kitchen Countertops

Cov khoom tseem ceeb

Nqe lus hauv qab no tham txog cov khoom ntawm qib 440 bar cov khoom lag luam hauv qab ASTM A276. Cov txiaj ntsig no yuav tsis zoo ib yam li lwm cov ntaub ntawv xws li forgings thiab phaj.

Kev sib xyaw

Cov tshuaj muaj pes tsawg leeg ntawm ntau yam khoom ntawm qib 440 stainless hlau yog tabulated hauv qab no:

Table 1. Cov tshuaj muaj pes tsawg leeg ntawm qib 440 stainless hlau

Qib

C

Mn

Si

P

S

Cr

Mo

Ni

N

440A

min.

max.

0.6

0.75

-

1

-

1

-

0.04

-

0.03

16

18

-

0.75

-

-

440B

min.

max.

0.75

0.95

-

1

-

1

-

0.04

-

0.03

16

18

-

0.75

-

-

440C

min.

max.

0.95

1.20

-

1

-

1

-

0.04

-

0.03

16

18

-

0.75

-

-

Mechanical Properties

Rooj 2.Mechanical zog ntawm qib 440C stainless hlau

Tempering kub (degree)

Tensile zog (MPa)

Yield Strength 0.2% Pov thawj (MPa)

Elongation (% hauv 50mm)

Hardness Rockwell (HR C)

Impact Charpy V (J)

Annealed *

758

448

14

269 ​​HB max #

-

204

2030

1900

4

59

9

260

1960

1830

4

57

9

316

1860

1740

4

56

9

371

1790

1660

4

56

9

* Annealed cov khoom yog raug rau Cov Mob A ntawm ASTM A276# Brinell hardness yog ASTM A276 teev siab tshaj plaws rau annealed 440A, B thiab C.

Lub cev muaj zog

Cov lus hauv qab no qhia txog lub cev lub cev ntawm qib 440 stainless hlau:

Table 3.Lub cev muaj zog ntawm qib 440 stainless hlau

Qib

Qhov ceev (kg / m3)

Elastic Modulus (GPa)

Lub ntsiab lus Coefficient ntawm Thermal Expansion (μm / m / degree)

Thermal conductivity (W / mK)

Thaum tshav kub kub
0-100degreeC (J/kg.K)

Hluav taws xob tiv thaiv (nΩ)

0-100 degree

0-200 degree

0-600 degree

ntawm 100 degree

ntawm 500 degree

440A/B/C

7650

200

10.1

10.3

11.7

24.2

-

460

600