Stainless Hlau Qib 316 - Muaj Corrosion Resistant

Feb 26, 2026

Tso lus

201 Stainless Steel Sheet for DecorationWhat is 1.4523 Stainless Steel?Stainless Steel - Grade 316 (UNS S31600)

 

Kev sib xyaw

Table 1.Kev sib xyaw ua ke rau qib 316 ntawm stainless hlau.

Qib CMnSiPSCrMoNiN
316Min---0-16.02.0010.0-
Max0.082.00.750.0450.0318.03.0014.00.10
316LMin-----16.02.0010.0-
Max0.032.00.750.0450.0318.03.0014.00.10
316HMin0.040.040--16.02.0010.0-
max0.100.100.750.0450.0318.03.0014.0-

 

Mechanical Properties

Rooj 2.Mechanical zog ntawm 316 qib stainless hlau.

QibTensile Str (MPa) minYield Str 0.2% Pov thawj (MPa) minNtev (% hauv 50 mm) minHardness
Rockwell B (HR B) maxBrinell (HB) max
3165152054095217
316L4851704095217
316H5152054095217

 

Nco tseg: 316H kuj tseem muaj qhov yuav tsum tau ua rau cov nplej loj ntawm ASTM tsis muaj . 7 lossis coarser.

Lub cev muaj zog

Table 3.Cov khoom siv lub cev zoo rau 316 qib stainless hlau.

QibQhov ceev (kg / m3)Elastic Modulus (GPa)Txhais tau tias Co-eff ntawm Thermal Expansion (µm/m/°C)Thermal conductivity (W / mK)Cov cua kub tshwj xeeb 0-100 ° C (J / kg.K)Elec Resistivity (nΩ)
0-100 ° C0-315 ° C0-538 ° CNtawm 100 ° CNtawm 500 ° C
316/L/H800019315.916.217.516.321.5500740

 

Qib Specification Sib piv

Table 4.Qib specifications rau 316 qib stainless hlau.

QibUNS NoLaus BritishEuronormSwedish SSJapanese JIS
BSEnTsis muajLub npe
316S31600316S3158H, 58J1.4401X5CrNiMo17-12-22347TIAB SA 316
316LS31603316S11-1.4404X2CrNiMo17-12-22348SUS 316L
316HS31609316S51-----