Qib SUS316L Stainless Hlau

Feb 27, 2026

Tso lus

Kev piav qhia

Qib SUS316L yog qhov qis-carbon variant ntawm SUS316, optimized los tiv thaiv intergranular corrosion tom qab vuam. Nrog cov ntsiab lus carbon txwv tsawg dua los yog sib npaug li 0.03%, nws zam chromium carbide nag lossis daus thaum lub sij hawm vuam, tswj kev tiv thaiv corrosion zoo heev hauv cov pob qij txha welded yam tsis tau tshaj tawm -weld heat treatment. Nws tau txais cov molybdenum- txhim kho corrosion kev ua tau zoo ntawm SUS316, ua rau nws muaj kev ntseeg siab hauv cov tshuaj chloride, tshuaj, thiab dej hiav txwv ib puag ncig-zoo dua rau 201 thiab txawm tias SUS304L. Tsis zoo li SUS316, SUS316L yog qhov kev xaiv zoo tshaj plaws rau cov khoom siv welded hnyav uas qhov ntev - lub sij hawm corrosion kuj yog qhov tseem ceeb, vim nws tshem tawm qhov xav tau rau kev tshaj tawm -weld annealing. Nws yog dav siv hauv kev lag luam uas cov khoom siv kev ncaj ncees tom qab vuam yog qhov tseem ceeb, muab qhov sib npaug ntawm kev tiv thaiv corrosion thiab kev ua haujlwm.

Chemical Composition (wt%)

C Tsawg dua lossis sib npaug 0.03, Cr: 16.00-18.50, Ni: 10.00-14.00, Mo: 2.00-3.00, Mn Tsawg dua lossis sib npaug 2.00, Si Less dua lossis sib npaug 1.00, P Less dua lossis sib npaug 0.04 lossis sib npaug 0.005,

Mechanical Properties

Tensile Strength Ntau dua los yog sib npaug rau 480 MPa, Yield Strength Ntau dua lossis sib npaug rau 175 MPa, Elongation Ntau dua lossis sib npaug li 40%, Hardness Tsawg dua lossis sib npaug rau 215 HB

Qhov zoo

Cov ncej zoo heev -weld corrosion kuj; superior rau SUS316 nyob rau hauv welded tej yam kev mob; khaws cov pitting siab nyob rau hauv chloride media; tsis yog-magnetic; zoo formability thiab weldability; corrosion ntau dua -resistant dua 201 thiab SUS304L.

Daim ntawv thov

Cov kav dej tshuaj, tso tsheb hlau luam, cov khoom siv hauv hiav txwv, cov khoom siv kho mob, cov tshuab siv tshuaj, cov khoom siv welded siab, thiab cov khoom siv nyob rau hauv qhov hnyav corrosive ib puag ncig.

Qib sib npaug

AISI 316L, UNS S31603, EN 1.4404, GB 022Cr17Ni12Mo2

 

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips