Qib 316Ti Stainless Hlau
316Ti yog titanium-stabilized variant ntawm 316L, ntxiv titanium los tiv thaiv chromium carbide nag lossis daus, kom ntseeg tau zoo heev intergranular corrosion kuj nyob rau hauv vuam thiab siab - kub ib puag ncig.
Chemical Composition (wt%):C Tsawg dua lossis sib npaug 0.08, Cr: 16.0-18.5, Ni: 10.0-14.0, Mo: 2.0-3.0, Ti: 5 × C-0.70, Mn Less dua lossis sib npaug 2.0, Si Less dua lossis sib npaug 1.0, P Less dua lossis sib npaug rau 0.04 lossis sib npaug
Mechanical Properties:Tensile zog Ntau tshaj los yog sib npaug rau 515MPa, Yield zog Ntau tshaj los yog sib npaug rau 205MPa, Elongation Ntau tshaj los yog sib npaug rau 40%, Hardness Tsawg dua los yog sib npaug rau 217 HB.
Kev Ua Haujlwm Zoo:Zoo siab -kub intergranular corrosion kuj tshaj 316/316L; tib pitting tsis kam raws li 316 series; ruaj khov dua 316L nyob rau hauv siab -kub corrosive tej yam kev mob.
Daim ntawv thov:Cov tshuaj reactors, lub tshuab tso pa, cov khoom siv hluav taws xob sib hloov, cov txheej txheem marine, siab -cov khoom siv corrosive welded.
Qib sib npaug:AISI 316Ti, UNS S31635, EN 1.4571, GB 06Cr17Ni12Mo2Ti.
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.


Xa kev nug