TS EN 1.4833 Austenitic Stainless Steel - Siab -Chromium Thaum tshav kub kub-Resistant Alloy

Feb 28, 2026

Tso lus

Kev piav qhia

EN 1.4833 yog siab -chromium austenitic stainless hlau, sib haum rau AISI 309S, tshwj xeeb yog tsim los rau siab - kub daim ntawv thov uas yuav tsum tau oxidation zoo heev. Nrog 22.0-24.0% chromium thiab 12.0-15.0% npib tsib xee, nws muaj kev tiv thaiv oxidation zoo tshaj ntawm qhov kub txog li 900 degree, ua tau zoo dua cov qauv qib zoo li EN 1.4301 hauv siab - cua sov ib puag ncig. Cov ntsiab lus carbon tsawg (tsawg dua lossis sib npaug li 0.08%) tiv thaiv kev nkag siab thiab txhim kho weldability, ua rau nws haum rau welded cov khoom kub kub. Tsis zoo li EN 1.4306, EN 1.4833 tseem ceeb rau oxidation tsis kam tshaj qhov kub thiab txias, ua rau nws zoo tagnrho rau cov khoom siv hluav taws xob, cov khoom siv hluav taws xob hloov hluav taws xob, thiab lwm yam khoom siv rau qhov kub thiab txias yam tsis muaj kev kub ntxhov.

Chemical Composition (wt%)

C Tsawg dua lossis sib npaug 0.08, Cr: 22.00-24.00, Ni: 12.00-15.00, Mn Tsawg dua lossis sib npaug 2.00, Si Less dua lossis sib npaug 1.00, P Tsawg dua lossis sib npaug 0.045, S Tsawg dua lossis sib npaug 0.030

Mechanical Properties

Tensile Strength Ntau dua los yog sib npaug rau 515 MPa, Yield Strength Ntau dua lossis sib npaug rau 205 MPa, Elongation Ntau dua lossis sib npaug li 40%, Hardness Tsawg dua lossis sib npaug rau 217 HB

Qhov zoo

Zoo heev - kub oxidation kuj (txog 900 degree); qis- carbon tsim rau zoo weldability; tsis yog-magnetic; zoo ductility thiab formability; resistant rau scaling nyob rau hauv siab -kub puag ncig; tus nqi- zoo rau kev siv cua sov- tiv taus.

Daim ntawv thov

Rauv hauv ob sab phlu, tshav kub exchangers, boiler qhov chaw, incinerator Cheebtsam, industrial cua sov ntsiab, thiab siab -kub ductwork.

Qib sib npaug

AISI 309S, UNS S30908, GB 06Cr23Ni13, SUS309S

 

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.