TS EN 1.4306 Stainless hlau - Tsawg-Carbon Weld-Sable General- Lub Hom Phiaj Alloy

Mar 25, 2026

Tso lus

Txheej txheem cej luam

EN 1.4306 yog qhov qis- carbon optimized variant ntawm EN 1.4301, nrog cov ntsiab lus carbon nruj tswj qis dua 0.03%. Tshwj xeeb tsim los daws cov teeb meem cuam tshuam ntawm intergranular thaum lub sij hawm vuam, nws yog qhov kev hloov kho ncaj qha rau cov qauv 304 qib hauv kev siv cov txheej txheem welded. Muab piv rau EN 1.4301, EN 1.4306 tshem tawm qhov kev pheej hmoo ntawm "sensitization" tshwm sim los ntawm kev tsim cov chromium carbides ntawm cov ciam teb nplej (tsim los ntawm kev sib xyaw ntawm carbon thiab chromium), kom tsis txhob muaj kev nyuaj siab -weld annealing yog yuav tsum tau thaum tuav lub qub corrosion kuj.

Chemical Composition (wt%)

C Tsawg dua lossis sib npaug 0.03, Cr: 18.00-20.00, Ni: 8.00-11.00, Mn Tsawg dua lossis sib npaug 2.00, Si Less dua lossis sib npaug 1.00, P Less dua lossis sib npaug 0.045, S Less dua lossis sib npaug 0.015, sib npaug

Tej yam cuab yeej cuab tam (Annealed Condition)

Tensile Strength (Rm): Ntau dua lossis sib npaug li 480 MPa; Yield zog (Rp0.2): Ntau dua lossis sib npaug ntawm 175 MPa; Elongation (A): Ntau dua lossis sib npaug li 40%; Brinell Hardness (HB): Tsawg dua lossis sib npaug rau 201

Core Zoo

Sensitization-tiv thaiv tsim: cov ntsiab lus tsis tshua muaj cov pa roj carbon tsawg ua kom muaj kev ruaj ntseg corrosion nyob rau hauv tshav kub- cuam tshuam cheeb tsam thaum vuam, hauv paus tshem tawm intergranular corrosion txaus ntshai; txheej txheem simplification: tsis muaj ncej-weld tov annealing yuav tsum tau, txo nqi ntau lawm thiab cycles loj los yog complex welded qhov chaw; Kev tuav pov hwm kev ua tau zoo: muaj peev xwm txais tau qhov dav dav corrosion tsis kam thiab formability ntawm EN 1.4301.

Daim ntawv thov

Welded siab hlab ntsha, cov kav dej tshuaj, cov kav dej ua zaub mov, cov tso tsheb hlau luam loj, cov khoom siv welded nyob rau hauv ib puag ncig corrosive, thiab architectural welded qhov chaw.

Qib sib npaug

AISI 304L, UNS S30403, GB 022Cr19Ni10, SUS304L

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips

Xa kev nug