Dab tsi yog 409 Stainless Hlau Phaj & Coil?

409 stainless hlau phaj & coil yog ib qho qis -chromium ferritic stainless hlau khoom, featuring zoo heev formability thiab nqi kom zoo dua. Nws yog dav siv los ua ib qho dav dav - cov khoom siv rau kev lag luam thiab cov khoom siv tsheb, ua ntej kev lag luam thiab kev txhim kho corrosion yooj yim.

Qib sib npaug (Horizontal)

UNS: S40900|JIS: SUS409L|GB: 022Cr11Ti|EN: X2CrTi12|PIB: 1.4512

Chemical Composition (wt%, Kab rov tav)

C: Tsawg dua lossis sib npaug rau 0.03|Si: Tsawg dua lossis sib npaug rau 1.00|Mn: Tsawg dua lossis sib npaug rau 1.00|P: Tsawg dua lossis sib npaug rau 0.045|S: Tsawg dua lossis sib npaug rau 0.030|Cr: 10.50-11.75|Ti: 6 × C-0.75|Fe: Sib npaug

Cov khoom tseem ceeb (20 degree, Annealed, Kab rov tav)

Qhov ceev: 7.75g / cm³|Melting Point: 1425-1510 degree|Tensile Strength: Ntau dua lossis sib npaug rau 415N / mm²|Yield Strength: Ntau dua lossis sib npaug rau 205N / mm²|Elongation: Ntau dua lossis sib npaug li 20%|Hardness: Tsawg dua los yog sib npaug rau 183HB

Cov yam ntxwv tseem ceeb

• Tus nqi siab-kev ua tau zoo: Cov ntsiab lus chromium tsawg txo cov nqi tsim khoom, tsim rau loj- nplai dav dav siv hauv kev lag luam • Zoo heev formability thiab weldability: Yooj yim rau txiav, khoov, yob thiab vuam, yoog rau phaj / coil ua thiab cov khoom tsim khoom • Zoo siab- kub oxidation kuj: Haum rau nruab nrab{{3} kev tiv thaiv corrosion, daim ntawv tiv thaiv kab mob. Zoo tagnrho rau qhuav lossis qis- ib puag ncig cov av noo, dav siv nyob rau hauv lub tsheb tso tsheb thiab cov casings muaj

409 vs 430 Stainless Hlau Phaj & Coil ( Kab rov tav )

Cr Cov ntsiab lus: 409 (10.50-11.75%)|430 (16.00-18.00%)|Corrosion Resistance: 409 (Basic)|430 (Zoo)|Tus nqi: 409 (qis)|430 (Nruab nrab)|Daim Ntawv Thov: 409 (Automotive/General)|430 (Khoom / Chav ua noj)

 

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau cov phaj, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, lossis ntim raws li cov neeg siv khoom xav tau.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips

Xa kev nug