316 Stainless Hlau Phaj yog austenitic stainless hlau

Apr 14, 2026

Tso lus

SUS304 Austenitic Stainless Steel – Versatile Corrosion-Resistant Universal Alloy304 Stainless Steel Round Bar from GneeSUS304L Austenitic Stainless Steel – Low-Carbon Weld-Stable Corrosion SolutionSUS316 Austenitic Stainless Steel – Molybdenum-Enhanced Chloride-Resistant Alloy

Cov ntsiab lus lag luam

Cov ntsiab lus Specification
Yam tsawg kawg nkaus Order Quantity: 5 Tons
Nqe: Yuav tsum sib tham
Ntim Cov Lus Qhia:

Raws li thov

Lub sij hawm xa tuaj: Hauv 7-10 Hnub Ua Haujlwm
Cov nqe lus them nqi: T / T, L / C, Credit Card
Muaj peev xwm muab khoom: 100000 Tons ib hlis twg
Ntawv pov thawj: RoHS, BIS, SABS, tisi, KS, JIS, ISO9001
Export rau:

United States, United Kingdom, Australia, India, Kauslim Teb, Hong Kong, Lavxias Federation, Brazil, Malaysia, Canada, Philippines, United States, Indonesia, Israel, Afghanistan, Albania, Algeria, American Samoa, Andorra, Angola, AnguillaAntigua Thiab Barbuda, Argentina, Armenia, Austria, Azerbaijan, Bahamas, Bangladesh, Bellarusize, Belgium Bhutan, Bolivia, thiab lwm yam.

Tshuaj muaj pes tsawg leeg

Lub ntsiab Cov pa roj carbon (C) Chromium (Cr) Nickel (Ni) Manganese (Mn) Silicon (Si) Phosphorus (P) Sulfur (S) Molybdenum (hli) Nitrogen (N) Hlau (Fe)
                     
Ntau yam 0.08 max 16.0 – 18.0 10.0 – 14.0 2.0 max 1.0 max 0.045 max 0.03 max 2.0 – 3.0 0.10 max Tshuav

Mechanical Properties

Cov khoom Chav ntsuas ntsuas Imperial Unit
     
Tensile zog 515-690 MPa 74,700-100,000 psi
Yield zog 205 MPa 30,000 psi
Vickers Hardness 150-220 HV 150-220 HV
Brinell Hardness 146-217 IB 146-217 IB
Rockwell Hardness B80 – B95 B80 – B95
Elongation 40% 40%
Elastic Modulus 193-200 GPa 28,000 – 29,000 KSI

Kev kho cua sov

Sheet Plate Heat Treatment

Annealing

Kub: 1,040 - 1,120℃(1,900 - 2,050℃F)

Txheej Txheem: Rhaub thiab tom qab ntawd txias sai, feem ntau yog los ntawm huab cua lossis dej quenching

Kev ntxhov siab

Kub: 450 - 600℃(840 - 1,110℃F)

Txheej Txheem: Rhaub thiab ua raws li cua txias

Hardening

Tsawg dua

316 stainless hlau tsis tuaj yeem hardened los ntawm kev kho cua sov, tsuas yog ua haujlwm txias

Kev kho mob

Kub: 1,010 - 1,120℃(1,850 - 2,050℃F)

Txheej txheem: Rhaub thiab quenched kom yaj precipitates thiab txhim kho corrosion kuj