1. Cov European sib npaug ntawm AISI 316 yog dab tsi? EN 1.4401 (raws li EN 10095 tus qauv).

2. Suav qib 316 yog dab tsi? 06Cr17Ni12Mo2 (GB / T 1221 tus qauv).

3. Puas yog JIS muaj qhov sib npaug 316? Yog lawm, JIS SUS 316 (JIS G4303 tus qauv).

4. Qhov twg ASTM tus qauv npog 316 daim ntawv thiab daim hlau? ASTM A240 / ASME SA240.

5. Puas yog thoob ntiaj teb 316 qhov sib npaug sib pauv tau? Yog, nrog me me sib txawv ntawm impurity txwv ib tus qauv.316 Stainless Steel Pipe & TubeSUS631 Stainless Steel: Precipitation-Hardening for Spring ApplicationsSUS441 Stainless Steel: Ferritic Grade with Improved Corrosion Resistance