304 Stainless hlau: Lub Universal Workhorse rau General Corrosion Resistance

Apr 14, 2026

Tso lus

Txheej txheem cej luam:

304 stainless hlau, feem ntau hu ua 18/8 austenitic alloy, yog cov qib stainless hlau siv dav tshaj plaws hauv ntiaj teb. Nws yog ntau yam, tus nqi- kev xaiv zoo haum rau ntau yam kev siv dav dav, muab qhov sib npaug ntawm kev tsim, weldability, thiab corrosion kuj uas ua tau raws li kev lag luam thiab cov neeg siv khoom xav tau.

Chemical Composition (wt%):

Chromium (Cr): 18.0-20.0; Nickel (Ni): 8.0-11.0; Carbon (C): Tsawg dua lossis sib npaug rau 0.08; Manganese (Mn): Tsawg dua lossis sib npaug li 2.00; Silicon (Si): Tsawg dua lossis sib npaug rau 1.00; Phosphorus (P): Tsawg dua lossis sib npaug rau 0.045; Sulfur (S): Tsawg dua lossis sib npaug rau 0.030; Hlau (Fe): Sib npaug.

Tej yam cuab yeej cuab tam (Annealed Condition):

Tensile Strength: Ntau dua lossis sib npaug ntawm 515 MPa; Yield zog: Ntau dua lossis sib npaug ntawm 205 MPa; Elongation: Ntau dua lossis sib npaug li 40%; Hardness (Brinell): Tsawg dua lossis sib npaug rau 201 HB.

Core Zoo:

Tsis yog-magnetic; zoo heev formability thiab weldability, haum rau ntau yam kev ua (bending, stamping, vuam); zoo oxidation kuj nyob rau hauv tas mus li kev pab cuam mus txog 870 degree; txhim khu kev qha corrosion kuj nyob rau hauv atmospheric thiab feem ntau me me corrosive ib puag ncig; tus nqi- zoo thiab yooj yim muaj nyob rau hauv ntau hom (cov ntawv, kav, tuav, fittings).

Daim ntawv thov:

Cov khoom siv hauv chav ua noj thiab cov tais diav, kev tsim vaj tsev thiab cladding, cov khoom siv hauv tsev (cov tub yees, qhov cub), cov khoom siv ua zaub mov (storage tanks, conveyors), automotive trim parts, general equipment, water tanks, and decorative fixtures.

Qib sib npaug: UNS S30400; EN 1.4301; JIS SUS304; GB/T 06Cr19Ni10.

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.

1.4547 Stainless Steel sheets

Xa kev nug