2507 Super Duplex Stainless Steel - Superior Corrosion Resistance

Feb 26, 2026

Tso lus

316 Stainless Steel Sheet for Medical Equipment316 Stainless Steel Pipe for Marine Engineering304 Stainless Steel Profile - Building Decoration and Durability

Tshuaj muaj pes tsawg leeg

Cov tshuaj muaj pes tsawg leeg ntawm stainless hlau qib Super Duplex 2507 yog teev nyob rau hauv cov lus hauv qab no.

Element Cov ntsiab lus (%)
Chromium, Cr 24 – 26
Nickel, Nia 6 – 8
Molybdenum, Mo 3 – 5
Manganese, Mn 1.20 max
Silicon, Sib 0.80 max
tooj, Cu 0.50 max
Nitrogen, N 0.24 – 0.32
Phosphorus, P 0.035 max
Carbon, C 0.030 max
Sulfur, S 0.020 max
Hlau, Fe Tshuav

Lub cev muaj zog

Lub cev lub cev ntawm stainless hlau qib Super Duplex 2507 yog tabulated hauv qab no.

Cov khoom Metric Imperial
Qhov ntom 7.8g / cm33 0.281 lb/in3
Melting point 1350 degree 2460℃F

Daim ntawv thov

Super Duplex 2507 yog siv dav hauv cov haujlwm hauv qab no:

Hwj chim

Tubrog nkoj

Tshuaj

Pulp thiab ntawv

Petrochemical

Dej desalinization

Roj thiab roj ntau lawm

Cov khoom tsim siv Super Duplex 2507 suav nrog:

Kiv cua

Hlau

Fittings

Cargo tanks

Cov dej kub

Cov nkoj khaws cia

Hydraulic kav

Kub exchangers

Cov dej kub tank

Kauv qhov txhab gaskets

Lifting thiab pulley khoom

Cov rotors, rotors, thiab shafts